Polymer Property : Shear Strength = 3.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 3.93 MPa
570 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 3.93 MPa
570 psi
Overlap, Isopropyl Alcohol Wipe surface prep, FRP
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 3.93 MPa
570 psi
On Douglas Fir
3M Scotch-Weld™ 3789 Hot Melt Adhesive
High performance for plastics; Impact resistant; Bonds vinyl and wood and Good fuel and oil resistanceInformation provided by 3M
Shear Strength 3.93 MPa

@Temperature 121 °C,
Time 900 sec
570 psi

@Temperature 250 °F,
Time 0.250 hour
Aluminum Overlap
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 3.93 MPa
570 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..