Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.93 MPa | 570 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 3.93 MPa | 570 psi | Overlap, Isopropyl Alcohol Wipe surface prep, FRP |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 3.93 MPa | 570 psi | On Douglas Fir |
3M Scotch-Weld™ 3789 Hot Melt Adhesive High performance for plastics; Impact resistant; Bonds vinyl and wood and Good fuel and oil resistanceInformation provided by 3M |
|||
Shear Strength | 3.93 MPa @Temperature 121 °C, Time 900 sec |
570 psi @Temperature 250 °F, Time 0.250 hour |
Aluminum Overlap |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 3.93 MPa | 570 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |