Polymer Property : Shear Strength = 31.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 31.7 MPa
4600 psi
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy
Inexpensive utility solderInformation Provided by Indium Corporation
Shear Strength 31.7 MPa
4600 psi
Overlap, Methyl Ethyl Ketone immersion, RT for 30 days
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.7 MPa
4600 psi
Overlap, Aluminum, RT cure for 24 hrs; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 31.7 MPa
4600 psi
Overlap, Aluminum, 49°C for 2 hrs; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 31.7 MPa

@Temperature 81.0 - 83.0 °C
4600 psi

@Temperature 178 - 181 °F
Average
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 31.7 MPa
4600 psi
Aluminum, etched, Overlap, 30 day water soak, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 31.7 MPa
4600 psi
Aluminum, etched, Overlap, 30 day water soak, Cohesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..