Material Notes:
Inexpensive utility solderInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.28 g/cc
0.335 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 12
12
Tensile Strength at Break 37.2 MPa
5400 psi
Elongation at Break 25 %
25 %
Modulus of Elasticity 23.0 GPa
3340 ksi
Shear Strength 31.7 MPa
4600 psi
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 44.0 W/m-K

@Temperature 85.0 °C
305 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 183 - 238 °C
361 - 460 °F
Solidus 183 °C
361 °F
Liquidus 238 °C
460 °F
Component Elements Properties Metric English Comments
Lead, Pb 60 %
60 %
Tin, Sn 40 %
40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000170 ohm-cm
0.0000170 ohm-cm