Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 22.8 - 26.2 MPa | 3300 - 3800 psi | |
ND Industries SuperGlue Methyl 330 Low-Medium Viscosity - General purpose metal surfaceMeets military spec Mil-A-46050C Type I Class II |
|||
Shear Strength | 22.8 MPa | 3300 psi | Overlap, Etched Alum, 93°C/100% RH/2 wks |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 22.8 MPa | 3300 psi | Lap, Alum to Alum |
Atom Adhesives AA-BOND FS291 Epoxy Adhesive AA-BOND FS291 is a thixotropic room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its no-sag characteristics are critica.. |
|||
Shear Strength | 22.8 MPa | 3300 psi | Overlap, FR-4/FR-4 tested after 120°C/2 wks |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 22.8 MPa | 3300 psi | Overlap, Etched Al, Anti-icing Fluid at RT for 7 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 22.8 MPa | 3300 psi | Overlap, Etched Al, Hydrocarbon Fluid for 7 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 22.8 MPa | 3300 psi | Overlap, Etched Al, Salt Spray at RT for 30 days |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |