Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 34.5 MPa | 5000 psi | |
TriStar CJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, Etched Aluminum tested after 1 week of Immersion in Diesel fuel |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 34.5 MPa @Temperature 82.0 °C |
5000 psi @Temperature 180 °F |
Etched Aluminum Overlap |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |
|||
Shear Strength | 34.5 MPa @Temperature 24.0 °C |
5000 psi @Temperature 75.2 °F |
Etched Aluminum Overlap |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, Tap Water 30 days @ RT; ASTM D1002-72 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, 20% Salt Spray 30 days @ 35°C; ASTM D1002-72 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, 7 days at RT; ASTM D1002-72 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, Aromatic Fuels 7 days @ RT; ASTM D1002-72 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa @Temperature -55.0 °C |
5000 psi @Temperature -67.0 °F |
Overlap; ASTM D1002 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa @Temperature 24.0 °C |
5000 psi @Temperature 75.2 °F |
Overlap; ASTM D1002 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 34.5 MPa | 5000 psi | Overlap, Copper MEK/abrade/MEK |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |