Mechanical Properties Metric English Comments
Shear Strength 27.6 - 41.4 MPa
4000 - 6000 psi
ND Industries High Temperature SuperGlue 311
Very high viscosity with thermal cycling resistance
Shear Strength 27.6 MPa
4000 psi
NextGen Adhesives G907-25 Optical Epoxy Adhesive
Description: NGAC G907-25 is a low viscosity and clear adhesive system that is specifically formulated for optical and laser applications.Advantages and Applications: The NGAC G907-25 provides high ..
Shear Strength 27.6 MPa
4000 psi
Cured, tensile
Resin Technology Group CT-988 Cationic UV Cure Epoxy Adhesive
CT 988 is an epoxy-based, paste-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant,..
Shear Strength 27.6 MPa
4000 psi
Tensile
Resin Technology Group Fusion 509 Thixotropic Fusion Cyanoacrylate
Information provided by Resin Technology Group.
Shear Strength >= 27.6 MPa
>= 4000 psi
2 hours, 65°C
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Mix ratio 2 to 1 by volume.TIGA 202-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 202-EX offers a 20 minute pot life and good hardness development within..
Shear Strength 27.6 MPa
4000 psi
Resinlab® RC8048 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Shear Strength >= 27.6 MPa
>= 4000 psi
2 hours, 65°C
Resin Technology Group TIGA 216-EX High Performance Adhesive
Mix ratio 2 to 1 by volume.TIGA 216-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 216-EX offers a 60 minute pot life and good hardness development within..
Shear Strength 27.6 - 34.5 MPa
4000 - 5000 psi
ASTM D732
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Shear Strength 27.6 - 34.5 MPa
4000 - 5000 psi
ASTM D732
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Shear Strength 27.6 MPa
4000 psi
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Shear Strength 27.6 MPa
4000 psi
Short Beam
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta..
Shear Strength 27.6 MPa
4000 psi
Overlap, CRS Oakite degrease
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Overlap, Copper MEK/abrade/MEK
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Overlap, Copper MEK/abrade/MEK
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 27.6 MPa
4000 psi
Overlap, Brass CDA 260
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 27.6 MPa
4000 psi
Overlap, Stainless Steel MEK/abrade/MEK
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 27.6 MPa
4000 psi
Overlap, 50% Antifreeze for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 27.6 MPa
4000 psi
Overlap at 2 hrs after bonding
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 27.6 MPa

@Temperature 24.0 °C
4000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 27.6 MPa
4000 psi
Overlap, Etched Aluminum, Isopropanol at RT for 30 days immersion, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 27.6 MPa
4000 psi
Overlap, Aluminum-etched, Cohesive failure; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 27.6 MPa

@Temperature 23.0 °C
4000 psi

@Temperature 73.4 °F
Overlap, Aluminum
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 27.6 MPa
4000 psi
Aluminum, etched, Overlap, 30 day Gasoline soak, Cohesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..
Shear Strength 27.6 MPa

@Temperature -55.0 °C
4000 psi

@Temperature -67.0 °F
Overlap
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..
Shear Strength 27.6 MPa
4000 psi
Overlap, Aluminum Oakite degrease
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Overlap, Water Vapor, 49°C at 100% RH for 30 days
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Overlap, Water Vapor, 93°C at 100% RH for 14 days
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Overlap, Skydrol LD-4 immersion, 66°C for 30 days
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 27.6 MPa
4000 psi
Resinlab® RC8020 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Copyright © lookpolymers.com All Rights Reserved