Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 275.8 MPa | 40000 psi | Shear Bond Holding Strength |
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
Shear Strength | 276 MPa | 40000 psi | |
Meehanite GC-40 Flake Graphite Cast Iron Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d.. |
|||
Shear Strength | 276 MPa | 40000 psi | |
Wingate Alloys Winco CBS Steel Chockblocks, Buttons, Skidblocks Winco CBS delivers tough reliable, low cost wear protection. Products can be used singly or combined to form a pattern wear resistance to address high wear in heavy-duty applications. Conditions met.. |