Material Notes:
Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 14.51 g/cc
0.5242 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 275.8 MPa
40000 psi
Elongation at Break 2.0 %
2.0 %
Modulus of Elasticity 59.1 GPa
8570 ksi
Shear Strength 275.8 MPa
40000 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 °C
8.89 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.150 J/g-°C
0.0359 BTU/lb-°F
Solid
Thermal Conductivity 57.0 W/m-K

@Temperature 85.0 °C
396 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 280 °C
536 °F
Eutectic
Solidus 280 °C
536 °F
Liquidus 280 °C
536 °F
Component Elements Properties Metric English Comments
Gold, Au 80 %
80 %
Tin, Sn 20 %
20 %