Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 46.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 46.9 MPa

@Temperature 23.9 °C
6800 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Shear Strength 46.9 MPa

@Temperature 149 °C
6800 psi

@Temperature 300 °F
Greene Tweed Arlon® 1000 Polyketone
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Shear Strength >= 46.9 MPa
>= 6800 psi
Die
Epoxy Technology EPO-TEK® 323LP Epoxy
Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology
Shear Strength >= 46.9 MPa
>= 6800 psi
Die
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy
Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti..
Shear Strength >= 46.9 MPa
>= 6800 psi
Die
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy
Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in..
Shear Strength >= 46.9 MPa
>= 6800 psi
Die
Epoxy Technology EPO-TEK® OM125 Optical Epoxy
Product Description: EPO-TEK® OM125 is two component, high Tg, optical epoxy designed for bonding multi-mode fiber optic connectors. Advantages & Application Notes: Color coded blue for easy operat..
Shear Strength 46.9 MPa
6800 psi
Die
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy
Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo..
Shear Strength 46.9 MPa
6800 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C and 80% RH
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..