Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Epoxy Technology EPO-TEK® 323LP Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Epoxy Technology
Trade Name EPO-TEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Technology EPO-TEK® 323LP Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
Part B
1.20 g/cc
1.20 g/cc
Part A
Viscosity 3500 - 5000 cP

@Temperature 23.0 °C
3500 - 5000 cP

@Temperature 73.4 °F
50 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Tensile Modulus 2.67 GPa
388 ksi
Storage
Shear Strength >= 13.8 MPa
>= 2000 psi
Lap
>= 46.9 MPa
>= 6800 psi
Die
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C
17.2 µin/in-°F
Below Tg
132 µm/m-°C
73.3 µin/in-°F
Above Tg
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
350 °C
662 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 100 °C
>= 212 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 413 °C
775 °F
Degradation Temperature
Optical Properties Metric English Comments
Refractive Index 1.5703

@Wavelength 589 nm
1.5703

@Wavelength 589 nm
Transmission, Visible <= 94 %

@Wavelength 820 - 1620 nm
<= 94 %

@Wavelength 820 - 1620 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity >= 3.00e+12 ohm-cm
>= 3.00e+12 ohm-cm
Dielectric Constant 2.62

@Frequency 1000 Hz
2.62

@Frequency 1000 Hz
Dissipation Factor 0.032

@Frequency 1000 Hz
0.032

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 90.0 °C
0.500 hour

@Temperature 194 °F
Pot Life 1440 min
1440 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear to Slight Yellow
Part A
Yellow
Part B
Consistency Pourable liquid
Mix Ratio By Weight 10:1
Number of Components Two
Weight Loss 0.31%
200°C
0.46%
250°C
0.85%
300°C