Mechanical Properties Metric English Comments
Shear Strength 32.1 MPa

@Temperature 23.0 °C
4650 psi

@Temperature 73.4 °F
Aluminum, Overlap
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 32.1 MPa
4650 psi
Etched Aluminum Overlap, Methyl Ethyl Keton, RT for 30 days immersion
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Shear Strength 32.1 MPa
4650 psi
Etched Aluminum Overlap Freon 22 Resistance, Control
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M
Shear Strength 32.1 MPa
4650 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in 50% Anitfreeze
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 32.1 MPa
4650 psi
Overlap, Etched Al, Air at 71°C for 35 days
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..