Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 47.0 MPa | 6820 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Shear Strength | 47.0 MPa @Temperature 93.0 °C |
6820 psi @Temperature 199 °F |
Compression interlaminar |
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel |
|||
Shear Strength | 47.0 MPa @Temperature 22.0 °C |
6820 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |