Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 53.1 MPa @Temperature 21.1 °C |
7700 psi @Temperature 70.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 53.1 MPa | 7700 psi | ASTM D732 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
Shear Strength | 53.1 MPa | 7700 psi | ASTM D732 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |