Mechanical Properties Metric English Comments
Shear Strength 53.1 MPa

@Temperature 21.1 °C
7700 psi

@Temperature 70.0 °F
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 53.1 MPa
7700 psi
ASTM D732
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications
Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe..
Shear Strength 53.1 MPa
7700 psi
ASTM D732
Quantum PEEK
Information provided by Quantum Advanced Engineering Plastics