Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Network Polymers Kepital® F20-52 Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Network Polymers Kepital® F40-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Shear Strength | 55.2 MPa @Temperature 23.9 °C |
8000 psi @Temperature 75.0 °F |
Short Beam; Dry; ASTM D695 |
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre.. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quadrant EPP Quadrant Nylon 612 |
|||
Shear Strength | 55.2 MPa @Temperature 288 °C |
8000 psi @Temperature 550 °F |
In-plane, Dry |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |
|||
Shear Strength | 55.2 - 82.7 MPa | 8000 - 12000 psi | Average value: 67.3 MPa Grade Count:4 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Shear Strength | 55.2 - 68.9 MPa | 8000 - 10000 psi | Die; Bare Si die on alumina |
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |
|||
Shear Strength | 55.2 MPa | 8000 psi | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Shear Strength | 55.2 - 62.1 MPa | 8000 - 9000 psi | ASTM D732 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |