Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.50 %
0.50 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Hardness, Rockwell R 126
126
ASTM D785
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength 110 MPa
16000 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Tensile Modulus 4.34 GPa
630 ksi
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Compressive Strength 138 MPa
20000 psi
10% Def.; ASTM D695
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Shear Strength 55.2 MPa
8000 psi
ASTM D732
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.32
0.32
Dry vs. Steel; QTM55007
K (wear) Factor 755 x 10-8 mm³/N-M
375 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.298 MPa-m/sec
8500 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 46.8 µm/m-°C

@Temperature -40.0 - 149 °C
26.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.252 W/m-K
1.75 BTU-in/hr-ft²-°F
ASTM F433
Melting Point 340 °C
644 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.9 kV/mm
480 kV/in
Short Term; ASTM D149
Dissipation Factor 0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Canada AG No
No
FDA Yes
Yes
NSF No
No
USDA Yes
Yes
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Color Natural
Machinability 5
1-10, 1=Easier to Machine
Users viewing this material also viewed the following: