Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 42.42 MPa | 6152 psi | Etched Aluminum Overlap, Tap Water @ RT for 180 days |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |