Polymer Property : Shear Strength = 7.24 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 7.24 MPa
1050 psi
CRS Overlap, 100% RH at 49°C
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Shear Strength 7.24 MPa
1050 psi
Overlap, Lexan, AF/CF
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 7.24 MPa
1050 psi
Overlap, ABS, Substrate Failure
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 7.24 MPa
1050 psi
Overlap, Plywood, Cohesive Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.24 MPa

@Temperature 32.0 °C
1050 psi

@Temperature 89.6 °F
Overlap, Plywood, 90% RH, Substrate Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.24 MPa
1050 psi
Overlap, Aluminum-MEK/abrade/MEK
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi..
Shear Strength 7.24 MPa
1050 psi
Overlap, Diesel Fuel, Substrate Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.24 MPa
1050 psi
Overlap, ABS, Substrate Failure
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 7.24 MPa
1050 psi
Overlap, Maple, Substrate Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.24 MPa

@Temperature 66.0 °C
1050 psi

@Temperature 151 °F
Overlap, Plywood, Substrate Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.24 MPa

@Temperature 66.0 °C
1050 psi

@Temperature 151 °F
Overlap, Aluminum, Adhesive Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.24 MPa
1050 psi
Overlap, Copper/Copper; ASTM D1002
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..