Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 7.943 MPa | 1152 psi | Lap |
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d.. |