Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 71.7 MPa | 10400 psi | Interlaminar, RT, Dry; ASTM D2344 |
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka.. |
|||
Shear Strength | 71.7 MPa | 10400 psi | Axial; ASTM D732 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 71.7 MPa | 10400 psi | Transverse; ASTM D732 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 71.7 MPa @Temperature 71.0 °C |
10400 psi @Temperature 160 °F |
Compression interlaminar |
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel |