Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.384 MPa | 1216 psi | Lap |
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos.. |