Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, MD = 0.0510 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.0510 GPa
7.40 ksi
2% Secant; ASTM D882
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina..
Copyright © lookpolymers.com All Rights Reserved