Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.146 GPa | 21.2 ksi | Film value |
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regul.. |