Polymer Property : Secant Modulus, MD = 0.207 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.207 GPa
30.0 ksi
1% Secant; ASTM D882
Eastman 1830F Polyethylene  (discontinued **)
Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and..
Secant Modulus, MD 0.207 GPa
30.0 ksi
1% Secant; ASTM D882
Eastman E6838-922F Polyethylene  (discontinued **)
E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
Huntsman PE1031 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
Huntsman PE1044 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
Huntsman PE1055 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms..
Secant Modulus, MD 0.207 GPa
30.0 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film
INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
Huntsman PE1061 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink..
Secant Modulus, MD 0.207 GPa
30.0 ksi
ASTM D882
Huntsman PE1158 EVA Film Extrusion  (discontinued **)
1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..