Polymer Property : Secant Modulus, MD = 21.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo..
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer.
Secant Modulus, MD 0.150 GPa
21.8 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging
The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan..
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin  (discontinued **)
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu..
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin  (discontinued **)
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E..
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin  (discontinued **)
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Secant Modulus, MD 0.150 GPa
21.8 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film
The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing ..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ISO 527-3
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Secant Modulus, MD 0.150 GPa
21.8 ksi
1%; ASTM D882
Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
Secant Modulus, MD 0.150 GPa
21.8 ksi
2% Secant Modulus; ASTM-D882
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene
TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
Chevron Phillips Vytek™ V208A3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Secant Modulus, MD 0.150 GPa
21.8 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin  (discontinued **)
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu..
Secant Modulus, MD 0.150 - 0.896 GPa
21.8 - 130 ksi
Average value: 0.425 GPa Grade Count:5
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..