Mechanical Properties Metric English Comments
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer.
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer.
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer.
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Novapol® PF-Y821-D Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Good stiffness and machinability, good blocking resistance.Applications: Bags-on-roll, produce bags, garment film, trash bags.Data provided by the manufacturer.
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ISO 527-3
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin
Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation ..
Secant Modulus, MD 0.200 GPa
29.0 ksi
Film value
Dow AFFINITY™ HF 1030 Polyolefin Plastomer
AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,..
Secant Modulus, MD 0.200 GPa
29.0 ksi
Film value
Dow Elite® 5100 Linear Low Density Polyethylene
5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro..
Secant Modulus, MD 0.200 GPa
29.0 ksi
1%; ASTM D882
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
Secant Modulus, MD 0.200 GPa
29.0 ksi
1%; ASTM D882
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces..
Secant Modulus, MD 0.200 GPa
29.0 ksi
value @ 0.1 mm/mm-min Initial strain rate; ASTM D-882
Bapolene® 222F Polyethylene, Film Grade
Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo..
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer.
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer.