Polymer Property : Secant Modulus, MD = 344 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 2.37 GPa
344 ksi
ASTM D882
Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS)
Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties.Features: Flame Retardant; Good Chemical Resistance; Good Elect..