Mechanical Properties Metric English Comments
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman PE5020 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms t..
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman PE1501 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa..
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman PE1503 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman PE1504 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman PE1507 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, TD 0.138 GPa
20.0 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners
INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens,..
Secant Modulus, TD 0.138 GPa
20.0 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 917 Monolayer Bonding Film
INTEGRAL 917 Adhesive Film is a single layer adhesive film for use where a higher flow rate and lower melt point are required. It is useful for bonding heat sensitive materials, or for porous subst..
Secant Modulus, TD 0.138 GPa
20.0 ksi
ASTM D882
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in..
Copyright © lookpolymers.com All Rights Reserved