Mechanical Properties Metric English Comments
Secant Modulus, TD 0.170 GPa
24.7 ksi
at 1%; ASTM D882
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ISO 5527
Total Finathene® LL 4010 FE 18 LLDPE film  (discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ISO 5527
Total Finathene® LL 4010 FH 18 LLDPE film  (discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ASTM D882
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ASTM D882
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ASTM D882
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac..
Secant Modulus, TD 0.170 GPa
24.7 ksi
ASTM D882
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne..
Secant Modulus, TD 0.170 GPa
24.7 ksi
2% Secant Modulus; ASTM-D882
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene
TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h..
Secant Modulus, TD 0.170 GPa
24.7 ksi
2% Secant Modulus; ASTM-D882
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene
TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l..
Secant Modulus, TD 0.170 GPa
24.7 ksi
2% Secant Modulus; ASTM-D882
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene
TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR..
Secant Modulus, TD 0.170 GPa
24.7 ksi
2% Secant Modulus; ASTM-D882
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad..
Secant Modulus, TD 0.170 GPa
24.7 ksi
at 1%; ASTM D882
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin  (discontinued **)
Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but ..