Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | at 1%; ASTM D882 |
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ISO 5527 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ISO 5527 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ASTM D882 |
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ASTM D882 |
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ASTM D882 |
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | ASTM D882 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad.. |
|||
Secant Modulus, TD | 0.170 GPa | 24.7 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin
(discontinued **) Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but .. |