Mechanical Properties Metric English Comments
Secant Modulus, TD 0.186 GPa
27.0 ksi
ASTM D882
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Secant Modulus, TD 0.186 GPa
27.0 ksi
ASTM D882
Huntsman PE1068 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21..
Secant Modulus, TD 0.186 GPa
27.0 ksi
Film value
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece..
Secant Modulus, TD 0.186 GPa
27.0 ksi
Film value
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece..
Secant Modulus, TD 0.186 GPa
27.0 ksi
ASTM D882
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Secant Modulus, TD 0.186 GPa
27.0 ksi
ASTM D882
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..