Mechanical Properties Metric English Comments
Secant Modulus, TD 0.100 - 0.450 GPa
14.5 - 65.3 ksi
Average value: 0.224 GPa Grade Count:63
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Secant Modulus, TD 0.130 - 0.450 GPa
18.9 - 65.3 ksi
Average value: 0.253 GPa Grade Count:57
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..