Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.100 GPa | 14.5 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Secant Modulus, TD | 0.100 GPa | 14.5 ksi | ASTM D882 |
ExxonMobil Escorene® LD-708 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal .. |
|||
Secant Modulus, TD | 0.100 - 0.450 GPa | 14.5 - 65.3 ksi | Average value: 0.224 GPa Grade Count:63 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |