Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.20 GPa | 174 ksi | ASTM D882 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Secant Modulus, TD | 1.20 GPa | 174 ksi | ASTM D882 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |