Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.276 - 1.379 GPa | 185.1 - 200.0 ksi | ASTM D882 |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Secant Modulus, TD | 1.172 - 1.379 GPa | 170.0 - 200.0 ksi | ASTM D882 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |