Secant Modulus, TD 0.448 - 1.55 GPa
65.0 - 225 ksi
Average value: 1.18 GPa Grade Count:15
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..