Polymer Property : Secant Modulus, TD = 65.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.448 - 1.55 GPa
65.0 - 225 ksi
Average value: 1.18 GPa Grade Count:15
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Secant Modulus, TD 0.448 - 0.586 GPa
65.0 - 85.0 ksi
ASTM D882
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film  (discontinued **)
Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell.
Secant Modulus, TD 0.448 - 0.586 GPa
65.0 - 85.0 ksi
ASTM D882
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film  (discontinued **)
Description: ACLAR® Cx™ 8A is a heat sealable coextruded CTFE film.Information provided by Honeywell.