Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.40 GPa | 203 ksi | Tangent; ASTM D882 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Secant Modulus, TD | 1.40 GPa | 203 ksi | Tangent; ASTM D882 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |