Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LF-0718-A LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: processing aid additiveCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPEApplications: thick or t.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion, food and liquid packaging.Data provided by the manufacturer.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ISO 5527 |
Total Finathene® LL 6010 FH 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ISO 5527 |
Total Finathene® LL 6010 FE 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips 2151 High Impact, Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Medium Slip, High Antiblock, Low Blocking and Good Openability, Good ProcessabilityApplications:Trash bags and other linersProcessing Co.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-B Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Trash bags, liners, general packaging.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Industrial liners, heavy duty bags.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Secant Modulus, TD | 0.200 - 0.230 GPa | 29.0 - 33.4 ksi | Average value: 0.208 GPa Grade Count:4 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | |
UBE 5033B Air Blown Nylon 6/66 Film Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | |
UBE 5034FDX17 Air Blown Nylon 6/66 Film Specialties: Special grade for Air blownLow curlHigh transparencyHigh shrinkGood thermoform-abilityApplications: Best for Air BlownProcessing: Pouch (Air blown)Information provided by UBE. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11H1 LLDPE Film Resin
(discontinued **) Low gel, Excellent heat sealability, Easy processability, High toughness and strengthApplications: Heavy duty sack, High strength packagingAdditives: Process stabilizer, Polymer process aid, Antiblo.. |
|||
Secant Modulus, TD | 0.200 GPa | 29.0 ksi | at 1%; ASTM D882 |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |