Mechanical Properties Metric English Comments
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman 1810F Polyethylene  (discontinued **)
Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt..
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman D4004-F Polyethylene  (discontinued **)
Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o..
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman D4008-F Polyethylene  (discontinued **)
Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac..
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman E6838-969F Polyethylene  (discontinued **)
E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap...
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman D4052-F Polyethylene  (discontinued **)
D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance...
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Eastman E6838-975F Polyethylene  (discontinued **)
E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film..