Polymer Property : Secant Modulus, TD = 476.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 2.275 - 3.282 GPa
330.0 - 476.0 ksi
ASTM D882
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo..