Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 2.275 - 3.45 GPa | 330.0 - 500 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Secant Modulus, TD | 2.275 - 3.28 GPa | 330.0 - 476 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Secant Modulus, TD | 2.275 - 3.45 GPa | 330.0 - 500 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Secant Modulus, TD | 2.275 - 3.45 GPa | 330.0 - 500 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Secant Modulus, TD | 2.275 - 3.28 GPa | 330.0 - 476 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Secant Modulus, TD | 2.275 - 3.448 GPa | 330.0 - 500.1 ksi | ASTM D882 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |
|||
Secant Modulus, TD | 2.275 - 3.282 GPa | 330.0 - 476.0 ksi | ASTM D882 |
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo.. |
|||
Secant Modulus, TD | 2.275 - 3.241 GPa | 330.0 - 470.1 ksi | ASTM D882 |
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro.. |