Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.462 GPa | 67.0 ksi | 2% Secant; ASTM D882 |
Dow XU 66129.00 Developmental Monolayer Adhesive Film XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid ure.. |