Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 99.0 °C
210 °F
Sealing Initial Temperature
Braskem Flexus® 9210 LLDPE Blown Film Extrusion  (discontinued **)
25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem
Heat Seal Strength Initiation Temperature 99.0 °C
210 °F
2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow ELITE™ 5400G Enhanced Polyethylene Resin
™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc..
Heat Seal Strength Initiation Temperature 99.0 °C
210 °F
Sealing Initial Temperature
Braskem Flexus® 9200 LLDPE Blown Film Extrusion
Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing ..