Polymer Property : Tenacity = 0.526 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.351 - 0.526 N/tex
3.98 - 5.96 g/denier
EMS-Griltech Grilon® BM 10 Nylon 6 Monofilament (Medium-Set)
Description: GRILON BM 10 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Tenacity 0.439 - 0.526 N/tex
4.97 - 5.96 g/denier
EMS-Griltech Grilon® BM 20R Nylon 6 Monofilament (Medium-Set)
Description: GRILON BM 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Tenacity 0.439 - 0.526 N/tex
4.97 - 5.96 g/denier
EMS-Griltech Grilon® BN 19 Nylon 6 Monofilament (Non-Set)
Description: GRILON BN 19 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Tenacity 0.351 - 0.526 N/tex
3.98 - 5.96 g/denier
EMS-Griltech Grilon® BN 20R Nylon 6 Monofilament (Non-Set)
Description: GRILON BN 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.