Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 1.15 N/tex | 13.0 g/denier | Tensile Modulus |
UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=4.5) Specialties: High viscosity Nylon 6/66 Copolymer, Higher transparent and softness than 5033T, High tenacity Applications: Small size sport fishing line and long- line (main line)Information provided.. |
|||
Tenacity | 1.15 N/tex | 13.0 g/denier | Tensile Modulus |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 2 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |
|||
Tenacity | 1.15 N/tex | 13.0 g/denier | Tensile Modulus |
UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=5.5) Specialties: High viscosity Nylon 6/66 Copolymer, Higher transparent and softness than 5033T, High tenacity Applications: Small size sport fishing line and long- line (main line)Information provided.. |
|||
Tenacity | 1.15 N/tex | 13.0 g/denier | Tensile Modulus |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 2 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |