UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=5.5)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=5.5).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialties: High viscosity Nylon 6/66 Copolymer, Higher transparent and softness than 5033T, High tenacity Applications: Small size sport fishing line and long- line (main line)Information provided by UBE.
Physical Properties Metric English Comments
Fiber Count 37000 dtex
33300 denier
Mechanical Properties Metric English Comments
Elongation at Break 33 %
33 %
Line Elongation
35 %
35 %
Knot Elongation
Tenacity 0.380 N/tex
4.30 g/denier
Knot Strength
0.609 N/tex
6.90 g/denier
Line Strength
1.15 N/tex
13.0 g/denier
Tensile Modulus
Thermal Properties Metric English Comments
Shrinkage 24 %
24 %
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified