Mechanical Properties Metric English Comments
Tenacity 0.353 N/tex
4.00 g/denier
Shakespeare MX-201 PP Polypropylene Monofilament
Generally good chemical resistance. Good biological resistance.Information provided by Shakespeare Company.
Tenacity 0.353 N/tex
4.00 g/denier
Shakespeare Resistat® F901 D044 Nylon 6 Monofilament
Resistat F901, MERGE D044 is a 44-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of ..
Tenacity 0.353 N/tex
4.00 g/denier
Shakespeare Resistat® F901 N022 Nylon 6 Monofilament
Resistat F901, MERGE N022 is a 22-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of ..
Tenacity 0.353 N/tex
4.00 g/denier
Shakespeare Resistat® F901 S022 Nylon 6 Monofilament
Resistat F901, MERGE S022 is a 33-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of ..
Tenacity 0.353 N/tex
4.00 g/denier
Shakespeare Resistat® F9122 A400 Nylon 6 Monofilament
Resistat F9122, MERGE A400 is a 22 denier per filament, 4 inch, conductive nylon 6 stable. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cr..
Tenacity 0.353 N/tex
4.00 g/denier
5 kg breaking load
Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Tenacity 0.353 N/tex
4.00 g/denier
Knot Strength
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5.5, Diameter 2 mm)
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic..