Shakespeare Resistat® F901 S022 Nylon 6 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Resistat® F901 S022 Nylon 6 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resistat F901, MERGE S022 is a 33-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of approximately 1 micron. The yarn color is black. Resistat is used for carpeting, ESD garments, and industrial belting and brushes.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Fiber Count 24.4 dtex
22.0 denier
Mechanical Properties Metric English Comments
Elongation at Break 41 %
41 %
Tenacity 0.353 N/tex
4.00 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Electrical Properties Metric English Comments
Electrical Resistivity 300000 ohm-cm
300000 ohm-cm